Advances in ultra-high-temperature ceramic coatings with enhanced oxidation resistance for carbon-based composites
Xuanru Ren, Peipei Wang, Yuexing Chen, Wei Xie, Xiang Ji, Zhichao Shang, Chengshan Ji, Jun Zhao, Huiqun Liu, Guozheng Lv, Peizhong Feng
Extreme Materials, 2025, 1(3): 9-43.   DOI: 10.1016/j.exm.2025.07.003

Fig. 19. Surface, cross-sectional morphology, and corresponding EDS analysis of ZS and ZSL coating samples after 550 h of oxidation at 1500C : (a) and (b) Secondary electron images of the surface of the ZS coating sample; (c) Backscattered electron image of the cross-section of the ZS coating sample; (d) and (e) Secondary electron images of the surface of the ZSL coating sample; (f) Backscattered electron image of the cross-section of the ZSL coating sample; (g) EDS area scan images of different elements corresponding to the cross-sectional morphology of the ZSL coating. Reproduced with permission from Ref. [110], © Elsevier 2018.